This material is made of polylactic acid (PLA), which is made with fermented plant starch by dehydrating, purifying, and polymerizing). The straw is mixed with 30% banana leaf fiber powder by granulation, and shaped by extrusion. Different from ordinary pure PLA, this material is compostable after disposal, and it can be decomposed faster under a specific conditions (50~60℃, RH 80~90%).more
You need to log in as a member to see the relevant information of the factory.
Member Login
Quick login
This material is made of polylactic acid (PLA), which is made with fermented plant starch by dehydrating, purifying, and polymerizing). The straw is mixed with 30% banana leaf fiber powder by granulation, and shaped by extrusion. Different from ordinary pure PLA, this material is compostable after disposal, and it can be decomposed faster under a specific conditions (50~60℃, RH 80~90%).